About: The study described poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) accumulation in Bacillus aryabhattai PHB10 for the first time and evaluated the polymer induced cytotoxicity in-vitro with PHBV/poly(ethylene glycol) (PEG) blends. The B. aryabhattai strain produced 2.8 g/L PHBV, equivalent to 71.15% of cell dry mass in a medium supplemented with propionic acid, after 48 h incubation. The optimum temperature and pH for the copolymer accumulation was 31 °C and 7, respectively. The gas chromatography–mass spectrometry and nuclear magnetic resonance analyses confirmed the polymer obtained as PHBV. The differential scanning calorimetry analysis revealed that the melting point of the material as 90 °C and its thermal stability up to 220 °C. The average molecular weight (Mn) and polydispersity index of the sample was estimated by gel permeation chromatography analysis and observed as 128.508 kDa and 2.82, respectively. The PHBV showed tensile strength of 10.3 MPa and elongation at break of 13.3%. The PHBV and their blends with PEG were tested for cytotoxicity on human keratinocytes (HaCaT cells) and the cells incubated with PHBV/PEG2kDa blends were 99% viable, whereas with the PHBV alone showed comparatively higher cytotoxicity. The significant improvement in the cell viability of PHBV/PEG2kDa blends indicates its potential as a candidate for skin graft applications.   Goto Sponge  NotDistinct  Permalink

An Entity of Type : fabio:Abstract, within Data Space : covidontheweb.inria.fr associated with source document(s)

AttributesValues
type
value
  • The study described poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) accumulation in Bacillus aryabhattai PHB10 for the first time and evaluated the polymer induced cytotoxicity in-vitro with PHBV/poly(ethylene glycol) (PEG) blends. The B. aryabhattai strain produced 2.8 g/L PHBV, equivalent to 71.15% of cell dry mass in a medium supplemented with propionic acid, after 48 h incubation. The optimum temperature and pH for the copolymer accumulation was 31 °C and 7, respectively. The gas chromatography–mass spectrometry and nuclear magnetic resonance analyses confirmed the polymer obtained as PHBV. The differential scanning calorimetry analysis revealed that the melting point of the material as 90 °C and its thermal stability up to 220 °C. The average molecular weight (Mn) and polydispersity index of the sample was estimated by gel permeation chromatography analysis and observed as 128.508 kDa and 2.82, respectively. The PHBV showed tensile strength of 10.3 MPa and elongation at break of 13.3%. The PHBV and their blends with PEG were tested for cytotoxicity on human keratinocytes (HaCaT cells) and the cells incubated with PHBV/PEG2kDa blends were 99% viable, whereas with the PHBV alone showed comparatively higher cytotoxicity. The significant improvement in the cell viability of PHBV/PEG2kDa blends indicates its potential as a candidate for skin graft applications.
Subject
  • Biochemistry
  • Polyesters
  • Amount of substance
  • Propionic acids
  • Copolymers
  • Biodegradable plastics
  • Bioplastics
  • Thermoplastics
part of
is abstract of
is hasSource of
Faceted Search & Find service v1.13.91 as of Mar 24 2020


Alternative Linked Data Documents: Sponger | ODE     Content Formats:       RDF       ODATA       Microdata      About   
This material is Open Knowledge   W3C Semantic Web Technology [RDF Data]
OpenLink Virtuoso version 07.20.3229 as of Jul 10 2020, on Linux (x86_64-pc-linux-gnu), Single-Server Edition (94 GB total memory)
Data on this page belongs to its respective rights holders.
Virtuoso Faceted Browser Copyright © 2009-2025 OpenLink Software